MCP HubMCP Hub
스킬 목록으로 돌아가기

troubleshoot-print-issues

pjt222
업데이트됨 Yesterday
4 조회
17
2
17
GitHub에서 보기
디자인ai

정보

이 Claude Skill은 접착 문제, 실틈 현상, 층간 어긋남과 같은 일반적인 3D 프린팅 실패를 체계적으로 진단하고 수정합니다. 이 기능은 출력물이 중간에 실패하거나 품질 결함이 나타날 때, 또는 하드웨어/재료 변경 후에 사용하도록 설계되었습니다. 이 스킬은 FDM 및 SLA 프린터에 대한 증상 분석을 통해 실행 가능한 문제 해결 방법을 제공합니다.

빠른 설치

Claude Code

추천
기본
npx skills add pjt222/agent-almanac -a claude-code
플러그인 명령대체
/plugin add https://github.com/pjt222/agent-almanac
Git 클론대체
git clone https://github.com/pjt222/agent-almanac.git ~/.claude/skills/troubleshoot-print-issues

Claude Code에서 이 명령을 복사하여 붙여넣어 스킬을 설치하세요

문서

Troubleshoot Print Issues

Diag + fix 3D print failures via systematic symptom analysis. Covers FDM + SLA: bed adhesion, stringing, layer shifts, warping, under-extrusion, over-extrusion, quality defects. Structured: ID symptom → root cause → iterative fix.

Use When

  • Print fails first layer|midway
  • Quality defects (stringing, blobs, gaps, rough surfaces)
  • Dim accuracy (over/undersized, warping, elephant foot)
  • Layer adhesion (delamination, splitting)
  • Support removal damages|supports fail
  • Prints differ from slicer preview
  • Material inconsistent across prints
  • New material|printer|env causing issues

In

  • failure_description: What went wrong (failed first layer, stringing, warping, etc.)
  • failure_timing: When (first layer, midprint, height, top)
  • material: Filament|resin type, brand, age, storage
  • printer: Make/model, nozzle size, bed type, enclosure
  • recent_changes: New material, slicer settings, hw mods, env
  • print_history: Model usually works? Material worked before?

Do

1. Collect Symptoms

Doc observable symptoms specifically:

Visual:

  • Photos (overall, close-up, defect)
  • Failure location (first layer, height, top)
  • Defect: gaps, blobs, strings, shifts, cracks

Env:

  • Ambient temp during print
  • Humidity
  • Drafts|AC
  • Time of day (temp changes)

Print params:

# Extract from G-code metadata
grep "^;MAXX\|^;MINX\|^;MAXZ" failed_print.gcode  # Print dimensions
grep "^;PRINT_TIME:" failed_print.gcode  # Estimated time
grep "^M104\|^M140" failed_print.gcode | head -5  # Temperatures
grep "^;generated by" failed_print.gcode  # Slicer version

Got: Detailed symptom desc w/ photos, params, env ctx.

If err: Symptoms unclear → print calibration test (temp tower, stringing test, benchy) → reproduce + observe systematically.

2. Classify by Pattern

Match symptoms → common failure modes:

Diagnostic Reference Table

SymptomLikely CausesQuick CheckPriority Fix
Poor bed adhesionDirty bed, wrong temp, too high ZWipe bed, level bedClean bed, adjust Z-offset down 0.05mm
StringingToo hot, insufficient retractionCheck nozzle tempLower temp 5°C, increase retraction +0.5mm
Layer shiftsLoose belts, too fast, collisionCheck belt tensionTighten belts, reduce speed 20%
WarpingPoor adhesion, fast coolingCheck corners liftingAdd brim, enclose printer, increase bed temp
Under-extrusionClog, low temp, wrong flowCheck extrusion consistencyClean nozzle, increase temp 5°C, calibrate e-steps
Over-extrusionHigh flow rate, wrong e-stepsCheck blob formationReduce flow 2-5%, calibrate e-steps
Elephant footFirst layer squish, bed too hotMeasure base widthRaise Z-offset +0.05mm, lower bed temp 5°C
Gaps in wallsThin walls, under-extrusionCheck wall thicknessEnable thin wall detection, increase flow
Layer delaminationLow temp, poor cooling, contaminationCheck layer linesIncrease temp 5-10°C, check wet filament
Blobs/zitsRetraction, coast settingsCheck seam alignmentTune retraction, enable coasting
Rough top surfaceInsufficient top layers, ironingCount solid top layersAdd 2 top layers, enable ironing
Sagging overhangsInsufficient cooling, too hotCheck part cooling fanIncrease cooling, lower temp, add supports

Got: Failure → 1-3 most likely categories.

If err: Multi categories → prioritize by failure timing (first layer first → midprint → top surface).

3. Root Cause Analysis

Investigate underlying cause, not just symptoms:

5 Whys:

Symptom: Print warping and lifting from bed
Why? → Poor bed adhesion in corners
Why? → Corners cooling faster than center
Why? → Room draft from AC vent
Why? → No enclosure to maintain stable temperature
Why? → ABS requires heated chamber for uniform cooling

Root cause: Material choice (ABS) incompatible with open printer in drafty room

Common root causes by category:

Mechanical:

  • Loose belts, pulleys, set screws
  • Worn|dirty linear bearings|rods
  • Z-axis binding|misalign
  • Extruder gear worn|skipping

Thermal:

  • Temp sensor drift|fail
  • Inadequate heated bed power|insulation
  • Insufficient part cooling
  • Env temp swings

Material:

  • Wet filament (hygroscopic)
  • Old|degraded
  • Contaminated (dust, oils)
  • Wrong material for app

Config:

  • Incorrect e-steps cal
  • Wrong flow rate multiplier
  • Slicer bug|wrong profile
  • Firmware accel|jerk too high

Got: Root cause ID'd w/ supporting evidence (measured temps, belt tension, visual).

If err: Root cause unclear → elimination: fix most likely → re-test → repeat.

4. First-Level Fixes

Poor Bed Adhesion

Immediate:

# 1. Clean bed thoroughly
# Glass/PEI: Isopropyl alcohol 90%+
# BuildTak: Warm water and dish soap

# 2. Level bed (paper test at 4 corners + center)
# Paper should drag slightly

# 3. Adjust Z-offset down (squish first layer more)
# Start: -0.05mm increments until lines fuse

# 4. Increase bed temperature +5°C

# 5. Add adhesion aid:
# - Glue stick (PLA/PETG)
# - Hairspray (ABS)
# - ABS juice (ABS) - ABS dissolved in acetone
# - Magigoo/3D printing adhesive

Slicer:

  • First layer height: 0.2-0.3mm (thicker = better squish)
  • First layer speed: 20mm/s (slower = better adhesion)
  • Brim: 8-10mm small footprint
  • Raft: difficult materials (TPU, Nylon)

Got: First layer adheres no lifting.

If err: Check bed flatness w/ feeler gauge|mesh level → warped bed needs glass/PEI or mesh comp.

Stringing

Temp-first:

1. Print temperature tower (180-220°C in 5° steps for PLA)
2. Identify lowest temperature that extrudes cleanly
3. Use that temperature -5°C to minimize stringing

Retraction:

# Direct drive extruder:
retraction_distance: 1.0-2.0mm
retraction_speed: 40-50mm/s

# Bowden extruder:
retraction_distance: 4.0-6.0mm
retraction_speed: 40-60mm/s

# If stringing persists:
- Enable z-hop: 0.2-0.4mm (lifts nozzle during travel)
- Reduce travel speed (paradoxically helps)
- Enable combing mode (travels within infill)

Got: Minimal stringing, thin strings hand-removable.

If err: Check nozzle partial clog|wet filament (both cause oozing).

Layer Shifts

Mech checks:

# 1. Check belt tension (should twang like guitar string)
# Tighten if loose

# 2. Check pulley set screws (motor shafts)
# Must align with flat on motor shaft

# 3. Check for mechanical resistance
# Manually move X/Y axes - should glide smoothly
# Binding indicates dirty rods, worn bearings, or misalignment

# 4. Check stepper motor current (advanced)
# Too low → skipping; too high → overheating

Speed reduction:

# Reduce these speeds:
perimeter_speed: 40mm/s (from 50)
travel_speed: 120mm/s (from 150)
acceleration: 500mm/s² (from 1000)
jerk: 8mm/s (from 15)

Got: No shifts in re-print w/ tightened belts + reduced speeds.

If err: Slicer-gen collisions (cooling fan hitting model)|electrical (stepper driver overheating).

Warping

Thermal:

# Increase bed temperature:
PLA: 60°C → 65°C
PETG: 80°C → 85°C
ABS: 100°C → 110°C

# Disable/reduce part cooling:
first_layer_fan: 0%
regular_fan: 25% max (ABS), 50% (PETG), 100% (PLA)

# Enclose printer (critical for ABS/ASA):
- Cardboard box (temporary)
- Acrylic panels (permanent)
- Target chamber temp: 40-50°C

Adhesion enhancement:

  • Brim: 10-15mm corners
  • "Mouse ears": 15mm discs at sharp corners
  • Chamfer bottom edges (45° × 1mm removes stress concentrator)

Got: Part stays flat, no corner lifting.

If err: Material unsuitable for printer (ABS unenclosed) → switch PETG|ASA.

Under-Extrusion

Quick:

# 1. Check for nozzle clog
# Heat to print temp, manually push filament
# Should extrude smoothly

# 2. Cold pull cleaning (if partial clog)
# Heat to 220°C, push cleaning filament through
# Cool to 90°C, pull sharply - should remove debris

# 3. Increase temperature +5-10°C
# Higher temp = better flow

# 4. Increase flow rate 2-5%
# Slicer: Filament settings → Flow → 102-105%

E-steps cal:

# 1. Mark filament 120mm above extruder
# 2. Extrude 100mm: G1 E100 F100
# 3. Measure remaining distance to mark
# 4. Calculate: new_steps = current_steps × (100 / actual_extruded)
# 5. Set: M92 E<new_steps>; M500 (save to EEPROM)

Got: Consistent extrusion, no gaps in perimeters|infill.

If err: Heat creep (cooling fan fail)|worn extruder gear|cracked extruder arm.

Over-Extrusion

Flow reduction:

# Reduce flow in 2% increments:
extrusion_multiplier: 0.98 → 0.96 → 0.94

# Signs of correct flow:
- Smooth top surface (not overstuffed)
- Perimeters don't bulge outward
- Infill doesn't overfill and push layers apart

Dim accuracy test:

# Print 20mm calibration cube
# Measure with calipers:
# X/Y dimensions should be 20.0mm ± 0.1mm
# If consistently oversized → reduce flow
# If undersized → increase flow

Got: Accurate dims, smooth surfaces, no bulging.

If err: Re-cal e-steps (may be too high).

5. Verify w/ Test Print

Confirm before full print:

Test selection:

  • Adhesion: 20mm sq × 5 layers (fast first layer test)
  • Stringing: Stringing test model (dual towers w/ travels)
  • Layer shifts: Tall thin (stress mechanical)
  • Warping: Large flat (200mm × 200mm × 0.4mm)
  • Extrusion: 20mm cal cube (dim accuracy)

Got: Test succeeds, issue resolved.

If err: Test fails → not fully resolved or multi issues → repeat diagnosis on remaining symptoms.

6. Doc Solution

Issue log template:

date: 2026-02-16
issue: "Layer shifts at 50mm height"
symptoms: "X-axis shifts 10mm, happens consistently at same height"
printer: "Ender 3 V2"
material: "PETG, PolyMaker PolyLite"
root_cause: "Loose X-axis belt, pulley set screw not on flat"
solution:
  - "Tightened X-axis belt to 120Hz resonance"
  - "Realigned pulley set screw on motor shaft flat"
  - "Reduced print speed to 40mm/s perimeter"
verification: "Printed 100mm test cylinder - no shifts"
notes: "Check belt tension monthly, pulley tends to slip"

Got: Issue documented w/ root cause + solution → knowledge base.

If err: Even unsuccessful attempts logged → avoid repeating failed solutions.

Check

  • Symptoms documented w/ photos + observations
  • Issue classified via diagnostic table
  • Root cause ID'd (mechanical, thermal, material, config)
  • Fix applied per root cause category
  • Fix verified w/ test print before full
  • Solution documented in issue log w/ date, cause, resolution
  • Env factors recorded (temp, humidity, drafts)
  • Material condition checked (dry, contamination-free, stored)

Traps

  1. Multi vars at once: One param at a time → otherwise won't know what fixed
  2. Ignore wet filament: Hygroscopic (Nylon, TPU, PETG) absorb moisture → bubbling, stringing, poor adhesion → suspect first
  3. Skip mech checks: Loose belts + worn parts cause issues no slicer tuning can fix
  4. Temp from internet: Every printer/material combo unique → run own temp tower
  5. Over-tighten belts: Too tight → premature bearing wear → guitar string tension, not steel cable
  6. Blame slicer: Bugs rare → 95% mechanical|thermal|material
  7. No clean nozzle: Partial clogs → intermittent under-extrusion looks like flow/e-step
  8. Assume bed level: Beds warp, springs compress, adjustments slip → re-level weekly
  9. Wrong Z-offset: Most first-layer fails = Z too high (no squish) or too low (scraping)
  10. Env neglect: ABS/ASA in 15°C garage w/ drafts won't print → needs stable warm

  • prepare-print-model: Properly prepared model → avoid printability issues
  • select-print-material: Material appropriate for printer + env
  • Calibrate 3D Printer (future): E-steps, flow rate, temp towers, PID tuning, bed mesh
  • Maintain 3D Printer (future): Belt tensioning, bearing lube, nozzle replace, preventive maint

GitHub 저장소

pjt222/agent-almanac
경로: i18n/caveman-ultra/skills/troubleshoot-print-issues
0
agentsagentskillsai-assisted-developmentclaude-codeskillsteams

연관 스킬

executing-plans

디자인

executing-plans 스킬은 검토 체크포인트가 포함된 통제된 배치로 실행할 완전한 구현 계획이 있을 때 사용합니다. 이 스킬은 계획을 불러와 비판적으로 검토한 후, 소규모 배치(기본값 3개 작업)로 작업을 실행하면서 각 배치 사이에 진행 상황을 아키텍트 검토를 위해 보고합니다. 이를 통해 내재된 품질 관리 체크포인트를 갖춘 체계적인 구현이 보장됩니다.

스킬 보기

requesting-code-review

디자인

이 스킬은 코드 변경 사항을 요구 사항에 따라 분석하기 위해 코드 리뷰어 하위 에이전트를 호출합니다. 작업 완료 후, 주요 기능 구현 후, 또는 메인 브랜치에 병합하기 전에 사용해야 합니다. 이 리뷰는 현재 구현체와 원래 계획을 비교하여 문제를 조기에 발견하는 데 도움이 됩니다.

스킬 보기

connect-mcp-server

디자인

이 스킬은 개발자들이 HTTP, stdio 또는 SSE 전송 방식을 통해 MCP 서버를 Claude Code에 연결하는 포괄적인 가이드를 제공합니다. GitHub, Notion 및 사용자 정의 API와 같은 외부 서비스를 통합하기 위한 설치, 구성, 인증 및 보안을 다룹니다. MCP 통합 설정, 외부 도구 구성 또는 Claude의 모델 컨텍스트 프로토콜 작업 시 활용하세요.

스킬 보기

web-cli-teleport

디자인

이 스킬은 작업 분석을 기반으로 개발자가 Claude Code 웹 인터페이스와 CLI 인터페이스 중 선택할 수 있도록 돕고, 두 환경 간 원활한 세션 텔레포트를 가능하게 합니다. 웹, CLI 또는 모바일 환경 전환 시 세션 상태와 컨텍스트를 관리하여 워크플로를 최적화합니다. 다양한 단계에서 서로 다른 도구가 필요한 복잡한 프로젝트에 사용하세요.

스킬 보기